Mechanical Properties Metric English Comments
Impact Test >= 40.0 J

@Temperature -40.0 °C
>= 29.5 ft-lb

@Temperature -40.0 °F
EN 10045-1
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Impact Test >= 40.0 J

@Temperature -40.0 °C
>= 29.5 ft-lb

@Temperature -40.0 °F
EN 10045-1
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Impact Test >= 40.0 J

@Temperature -40.0 °C
>= 29.5 ft-lb

@Temperature -40.0 °F
EN 10045-1
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS
FXC810MA is the grade code for the Marble effect in PC/ABS. Marble is part of the VisualFX portfolio, and it is offered in a range of colors simluating the Marble effect. High heat/good flow charact..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific)
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East)
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East)
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
Impact Test 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This ..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC
LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied..
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Impact Test 40.0 J
29.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DD000P PC
LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing.
Impact Test 40.0 J
29.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific)
LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing.
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific)
High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS
PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr..
Impact Test 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Instrumented, 15 mph; ASTM D3763
Phillips Sumika Marlex® CHP-055 Thermoplastic Polyolefin  (discontinued **)
Applications: Passenger-side Air--bag coverSoft interior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product ha..