Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 31.0 J

@Thickness 2.50 mm
22.9 ft-lb

@Thickness 0.0984 in
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Ineos ABS Lustran® 356 Extrusion, Low-Gloss  (discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Impact Test 31.0 J

@Thickness 2.50 mm
22.9 ft-lb

@Thickness 0.0984 in
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Ineos ABS Lustran® 552 Extrusion, Profile/Substrate
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Impact Test 31.0 J
22.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX93500 PC
LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Impact Test 31.0 J
22.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON MD000IS PP
LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Impact Test 31.0 J

@Temperature 5.00 °C
22.9 ft-lb

@Temperature 41.0 °F
Montell drop weight impact strength
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
Key Features: good impact and stiffness balance, good cold impact resistance, excellent dimensional stability, FDA acceptableApplications: corrugated board extrusion, appliancesMeets FDA requirement..
Impact Test 31.0 J
22.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Impact Test 31.0 J
22.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Impact Test 31.0 J
22.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..