Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 28.3 J @Temperature 23.0 °C |
20.9 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Magnum™ 9025 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |