Mechanical Properties Metric English Comments
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWE280 ASA
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer
Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX2415 PC
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer
Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 30.0 J

@Thickness 2.50 mm
22.1 ft-lb

@Thickness 0.0984 in
Instrumented Impact, Total Energy; 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Ineos ABS Lustran® 256 Extrusion, Blending  (discontinued **)
A natural, medium-flow, medium-impact extrusion grade of ABS. It is used for blending with other Lustran ABS virgin and regrind materials to optimize cost and performance.Properties tested in trans..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp DF002L PC
LNP THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the America..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 4455 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 30.0 J
22.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT
LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Impact Test 30.0 J

@Temperature -20.0 °C
22.1 ft-lb

@Temperature -4.00 °F
Total Penetration Energy; ISO 6603-2
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding
Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f..
Impact Test 30.0 J

@Thickness 3.20 mm
22.1 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Covestro Bayblend® T 45 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
Impact Test 30.0 J
22.1 ft-lb
Instrumented Impact; 20 mm width sample; ASTM D3763
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip
FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t..
Impact Test 30.0 J
22.1 ft-lb
63 mm diameter. Core strength in hardened condition.
Assab Steels 7210M Machinery Steel
ASSAB 7210M is an alloyed case hardening steel with high core strength.Applications: ASSAB 7210M is used for applications requiring a hard, wear resistant surface and a tough core, such as transmiss..
Impact Test 30.0 J

@Thickness 3.20 mm
22.1 ft-lb

@Thickness 0.126 in
Instrumented Impact, Total Energy; 3.2 mm thick, 2.5 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Bayblend® SF 1443 Polycarbonate + ABS Blend Structural Foam  (discontinued **)
Foam thickness 0.250 in. Properties values at foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from ..