Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.70 J | 1.99 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |