Polymer Property : Impact Test = 17.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 17.0 J
12.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66
LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region...
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA
Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta..
Impact Test 17.0 J
12.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly
LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic.
Impact Test 17.0 J
12.5 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 885 Profile Extrusion Grade
Centrex 885 resin is a low-gloss ASA (acrylonitrile-styrene-acrylate) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyviny..
Impact Test 17.0 J
12.5 ft-lb
ASTM D2794-93
3M Scotchkote™ 2400 Pipe Renewal Liner
NSF/ANSI-61 certified polyurea formulation is 100% solids and contains no epoxy resin. It is designed to help solve a wide variety of problems common to potable water systems. It utilizes a trenchle..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP
LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GFN1420V PPE+PS
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..