Mechanical Properties Metric English Comments
Impact Test 19.0 J
14.0 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Solvay Engineered Polymers SEQUEL® 1733HI Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1733HI engineered polyolefin is designed for large, painted automotive exterior applications that require dimensional stability over a broad temperature range. This material e..
Impact Test 19.0 J
14.0 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Solvay Engineered Polymers SEQUEL® 1880 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1880 engineered polyolefin is designed for large automotive applications that require dimensional stability over a broad temperature range. This material exhibits excellent pr..
Impact Test 19.0 J
14.0 ft-lb
Instrumented Impact Total Energy; ASTM D3763
ExxonMobil LD 513.48 Molding, Extrusion and Compounding Resin  (discontinued **)
LD 513.48 is a medium MI, low density polyethylene resin designed for use in compounds and masterbatches where its properties ensure improved processability and uniform dispersion of additives. The..
Impact Test 19.0 J

@Temperature -29.0 °C
14.0 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax SB912 Polypropylene Impact Copolymer
Key Features: fully formulated polypropylene copolymer resin, homopolymer-like stiffness wit improved impact strength, resist dust and dirt pick-up, excellent strengthApplications: closures, contain..
Impact Test 19.0 J

@Temperature -30.0 °C
14.0 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin
Key Features: fractional melt flow, medium low modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convolu..
Impact Test 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl PX7446 PPE+PS
This data was supplied by SABIC-IP for the Americas region.
Impact Test 19.0 J
14.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE
LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Impact Test 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Impact Test 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Impact Test 19.0 J
14.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
Impact Test 19.0 J
14.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Impact Test 19.0 J

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD2000 Polypropylene
DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E..
Impact Test 19.0 J

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD2000 Polypropylene
DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E..
Impact Test 19.0 J

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD2000 Polypropylene
DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E..
Impact Test 19.0 J

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD2000 Polypropylene
DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E..
Impact Test 19.0 J

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD2000 Polypropylene
DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E..
Impact Test 19.0 J

@Temperature -20.0 °C
14.0 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D3763
ExxonMobil LD 617.LN Molding, Extrusion and Compounding Resin
Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is..
Impact Test 19.0 J
14.0 ft-lb
@ 73ºF, Instrumented Impact Total Energy; ASTM D3763
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin
Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos..
Impact Test 19.0 J
14.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
Impact Test 19.0 J

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD2000 Polypropylene
DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E..
Impact Test 19.0 J
14.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Impact Test 19.0 J
14.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Stat-kon MDM40 PP
LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved