Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 16.9 - 22.6 J | 12.5 - 16.7 ft-lb | Torque Break |
Ritelok TL62 Studlock Anaerobic. High Strength studlock for heavy duty items, vibration & stress load. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Impact Test | 16.9 - 28.2 J | 12.5 - 20.8 ft-lb | Break |
ND Industries StudGrade® 131 Permanent CT Threadlocker General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m.. |
|||
Impact Test | 17.0 J | 12.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region... |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta.. |
|||
Impact Test | 17.0 J | 12.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Impact Test | 17.0 J | 12.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 885 Profile Extrusion Grade Centrex 885 resin is a low-gloss ASA (acrylonitrile-styrene-acrylate) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyviny.. |
|||
Impact Test | 17.0 J | 12.5 ft-lb | ASTM D2794-93 |
3M Scotchkote™ 2400 Pipe Renewal Liner NSF/ANSI-61 certified polyurea formulation is 100% solids and contains no epoxy resin. It is designed to help solve a wide variety of problems common to potable water systems. It utilizes a trenchle.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |