Polymer Property : Impact Test = 1.56 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 1.56 J
1.15 ft-lb
Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film
250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..