Polymer Property : Impact Test = 1.20 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 1.20 J
0.885 ft-lb
Instrumented Falling Weight Impact; ISO 6603/2
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot..