Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 0.700 J @Thickness 3.17 mm |
0.516 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc.. |
|||
Impact Test | 0.700 J @Thickness 3.17 mm |
0.516 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® KR01 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC can be processed by injection molding and extrusion into attractive useful parts that have excellent clarity, good toughness, good stiffness, h.. |