Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0280 GPa | 4.06 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
300% Modulus | 0.0280 GPa | 4.06 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0280 GPa | 4.06 ksi | ISO 37 |
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
300% Modulus | 0.0280 GPa | 4.06 ksi | ISO 37 |
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
300% Modulus | 0.0280 GPa | 4.06 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1495B Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0280 GPa | 4.06 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1495EC Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |