Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0140 GPa | 2.03 ksi | ISO 37 |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 H 4827 TPU-Polyester Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range .. |
|||
300% Modulus | 0.0140 GPa @Temperature 145 °C, Time 2990 sec |
2.03 ksi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 7150 High Acrylonitrile Polymer Description: NBR 7150 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 7150 is a non staining, medi.. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | ISO 37 |
Huntsman AVALON® 85 AB Thermoplastic Polyurethane Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
300% Modulus | 0.0140 - 0.0200 GPa | 2.03 - 2.90 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1507 Styrene Butadiene Rubber KRALEX® 1507 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin and fatty acids and contains 23.5% of chemical.. |
|||
300% Modulus | 0.0140 - 0.0190 GPa | 2.03 - 2.76 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1706 Styrene Butadiene Rubber KRALEX® 1706 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | DIN 53504 |
Lubrizol ESTANE® X4928 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | ISO 37 |
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | |
Lubrizol Estane® 54601 Thermoplastic Polyurethane Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in A.. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
300% Modulus | 0.0140 GPa | 2.03 ksi | ISO 37 |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |