Mechanical Properties Metric English Comments
300% Modulus 0.0101 GPa
1.46 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0101 GPa
1.46 ksi
Injection molded parts; ISO 37
Huntsman IROGRAN® A 80 H 4826 TPU-Polyester
Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and hig..
300% Modulus 0.0101 GPa
1.46 ksi
ASTM D412
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.0101 GPa
1.46 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0101 GPa
1.46 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4570 Dense Extruded Profile
FormulationNordel® IP 4570
300% Modulus 0.0101 GPa
1.46 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4570 General Purpose Compound
FormulationNordel® IP 4570