Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00890 GPa | 1.29 ksi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1161 P (SIS) Linear Triblock Copolymer Description: Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |