Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 1.10 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00758 GPa
1.10 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00755 GPa
1.10 ksi
Cured
KKPC KOSYN KBR 01 Polybutadiene Rubber (High cis BR)
Polybutadiene Rubber (High cis BR)Characteristics: Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solut..
300% Modulus 0.00758 GPa
1.10 ksi
Taiwan PU Corporation UR70 Polyester Urethane Rubber
UR70 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of ..
300% Modulus 0.00758 GPa
1.10 ksi
ASTM D412
SK Chemicals SKYTHANE® T875A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
300% Modulus 0.00755 GPa
1.10 ksi
ASTM D412
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane
Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Afr..
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio..
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast..
300% Modulus 0.00758 GPa
1.10 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.00758 GPa
1.10 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00758 GPa
1.10 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00758 GPa
1.10 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.00758 GPa
1.10 ksi
Forming
LG Chemical NBR 8300 High Acrylonitrile Polymer
Description: NBR 8300 is a copolymer of butadiene-acrylonitrile and the powdered nitrile elastomer manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 8300 has ..
300% Modulus 0.00758 GPa
1.10 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Copyright © lookpolymers.com All Rights Reserved