Mechanical Properties Metric English Comments
300% Modulus 0.00658 GPa
0.954 ksi
Injection molded parts; ASTM D412
Huntsman IROGRAN® CA116-201 TPU-Polyester
Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee..
300% Modulus 0.00658 GPa
0.954 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.00658 GPa
0.954 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..