Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00180 - 0.00390 GPa | 0.261 - 0.566 ksi | ASTM D 638 |
API Megol AM DP2154 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |