Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.276 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00190 GPa
0.276 ksi
ASTM D3574E
Mearthane Durethaneâ„¢ M DM-630A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
300% Modulus 0.00190 GPa
0.276 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1160 B (SIS) Linear Triblock Copolymer
Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kr..
300% Modulus 0.00190 GPa
0.276 ksi
ISO 37
Kraton® D42070 B (O/E SBS) Branched Copolymer
Description: Kraton® D4270B is an oiled, branched copolymer based on styrene and butadiene with a polystyrene content of 32%. It is supplied from South America in the physical form identified: D4..
300% Modulus 0.00190 GPa
0.276 ksi
ISO 37
Kraton® D4270 J (O/E SBS) Branched Block Copolymer
Description: Kraton D4270 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene in the neat polymer of 32% mass. It is supplied from Japan in the physical ..
300% Modulus 0.00190 GPa
0.276 ksi
ASTM D412
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti..
Copyright © lookpolymers.com All Rights Reserved