Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000392 GPa | 0.0569 ksi | JIS K6301 |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000392 GPa | 0.0569 ksi | JIS K6301 |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000392 GPa | 0.0569 ksi | JIS K6301 |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
300% Modulus | 0.000392 GPa | 0.0569 ksi | JIS K6301 |
Stellarchem MP-845B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000392 GPa | 0.0569 ksi | JIS K6301 |
Stellarchem MP-950NC TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000392 GPa | 0.0569 ksi | JIS K6301 |
Stellarchem 475-845N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |