Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0330 GPa | 4.79 ksi | ISO 37 |
Huntsman AVALON® 65 DE Thermoplastic Polyurethane Introduction: AVALON 65 DE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DE is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
300% Modulus | 0.0330 GPa | 4.79 ksi | ISO 37 |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
300% Modulus | 0.0330 GPa | 4.78 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0330 GPa | 4.79 ksi | ISO 37 |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |