Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0110 GPa | 1.59 ksi | ASTM D412 |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | 25 mil film; ASTM D412 |
Huntsman IROGRAN® A 95 P 5003 TPU-Polyether IROGRAN® A 95 P 5003 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers |
|||
300% Modulus | 0.0110 GPa @Temperature 145 °C, Time 2100 sec |
1.59 ksi @Temperature 293 °F, Time 0.583 hour |
ASTM D412 |
LG Chemical SBR 1723 High Acrylonitrile Polymer Description: SBR 1723 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 23.5% bound styrene. Raw materials for this p.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | DIN 53504 |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
300% Modulus | 0.0110 GPa | 1.59 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ISO 37 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1485RV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D412 |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
ELASTO UK Dryflex® 420451S SBS Based Material, 45D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | ASTM D638 |
ELASTO UK Dryflex® 422451S SBS Based Material, 45D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770P General Purpose Compound FormulationNordel® IP 4770P |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R General Purpose Compound FormulationNordel® IP 4770R |
|||
300% Modulus | 0.0110 GPa | 1.60 ksi | Compounded, 35 mins.; ISO 37 |
Dynasol Calprene® 375 Solution Random SBR Calprene 375 is a Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%, and is extended with 37.5 phr of naphthenic oil. C-375 is used .. |
|||
300% Modulus | 0.0110 GPa | 1.59 ksi | ASTM D412 |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
300% Modulus | 0.0110 GPa | 1.59 ksi | ASTM D412 |
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi.. |
|||
300% Modulus | 0.0110 GPa | 1.59 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0110 GPa @Temperature 145 °C, Time 2100 sec |
1.59 ksi @Temperature 293 °F, Time 0.583 hour |
ASTM D412 |
LG Chemical SBR 1723H High Acrylonitrile Polymer Description: SSBR 1723H is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 23.5% bound styrene. Raw materials for this.. |