Polymer Property : 300% Modulus = 0.00890 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00890 GPa
1.29 ksi
Measured on films cast from a solution in toluene; ASTM D412
Kraton® D1161 P (SIS) Linear Triblock Copolymer
Description: Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:..