Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00660 GPa | 0.957 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00660 GPa | 0.957 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00660 GPa | 0.957 ksi | ASTM D412 |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,.. |
|||
300% Modulus | 0.00660 GPa | 0.957 ksi | ISO 37 |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |