Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00621 GPa | 0.900 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.0 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00621 GPa | 0.901 ksi | ASTM D412 |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | |
Taiwan PU Corporation UR90 Polyester Urethane Rubber UR90 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2890M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.0 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00621 GPa | 0.900 ksi | ASTM D412 |
Lubrizol Estane® ALR PC73A Thermoplastic Polyurethane Type: Estane® ALR PC73A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |