Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00565 GPa | 0.820 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 65A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00565 GPa | 0.820 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 65A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |