Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00350 GPa | 0.508 ksi | ISO/R527 |
Polykemi AB POLYelast TPE E606 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00350 GPa | 0.508 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL TH 2315 Styrene - Ethylene / Butylene Block Copolymer Europrene® SOL TH 2315 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where b.. |
|||
300% Modulus | 0.00350 GPa | 0.508 ksi | ISO 37 |
Termopol Termoton® V2GA1065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
300% Modulus | 0.00350 GPa @Temperature 23.0 °C |
0.508 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 12 mil - Black, Ohio |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
300% Modulus | 0.00350 GPa | 0.508 ksi | ASTM D 638 |
API Megol AM DP2217/60PBT SEBS Adhesion Modified Overmolding for Polyesters Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |