Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00190 GPa | 0.276 ksi | ASTM D3574E |
Mearthane Durethaneâ„¢ M DM-630A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
300% Modulus | 0.00190 GPa | 0.276 ksi | Measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1160 B (SIS) Linear Triblock Copolymer Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kr.. |
|||
300% Modulus | 0.00190 GPa | 0.276 ksi | ISO 37 |
Kraton® D42070 B (O/E SBS) Branched Copolymer Description: Kraton® D4270B is an oiled, branched copolymer based on styrene and butadiene with a polystyrene content of 32%. It is supplied from South America in the physical form identified: D4.. |
|||
300% Modulus | 0.00190 GPa | 0.276 ksi | ISO 37 |
Kraton® D4270 J (O/E SBS) Branched Block Copolymer Description: Kraton D4270 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene in the neat polymer of 32% mass. It is supplied from Japan in the physical .. |
|||
300% Modulus | 0.00190 GPa | 0.276 ksi | ASTM D412 |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti.. |