Mechanical Properties Metric English Comments
300% Modulus 0.001103 GPa
0.1600 ksi
Measured on films cast from a solution in toluene; ASTM D412
Kraton® D4150 K (O/E SBS) Linear Triblock Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..