Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 65.5 MPa | 9500 psi | Steel-Steel; after optimum cure |
Armstrong A-701 Epoxy Adhesive A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond.. |