Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 5.52 MPa | 800 psi | Cast aluminum substrate 20 min @ 150°C (MT); ASTM D1002 |
Dow BETADAMP™ 32HT
(discontinued **) BETADAMP™ 32HT is a high temperature vibration damper that can be applied to the exterior of cast aluminum or steel engine valve, transmission, and crankcase (oil pan) covers or electro-coat substr.. |
|||
Adhesive Bond Strength | >= 5.52 MPa | >= 800 psi | shear, Al/Al, after 30 days water immersion |
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Adhesive Bond Strength | >= 5.52 MPa | >= 800 psi | shear, Al/Al, after 30 days water immersion |
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Adhesive Bond Strength | >= 5.52 MPa | >= 800 psi | shear, Al/Al, after 30 days water immersion |
Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy Master Bond Polymer System EP21TDCS MED is a two component, silver filled, electrically conductive adhesive/sealant that meets USP Class VI specifications for medical applications. The high strength.. |
|||
Adhesive Bond Strength | >= 5.52 MPa | >= 800 psi | After 30 days water immersion |
Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or .. |
|||
Adhesive Bond Strength | >= 5.52 MPa | >= 800 psi | After 30 days water immersion |
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit.. |
|||
Adhesive Bond Strength | 5.52 MPa | 800 psi | Lap shear, gold to gold, 45 min @ 150°C |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Adhesive Bond Strength | 5.52 MPa | 800 psi | Lap shear, glass to glass |
Tra-Con Tra-Coat WCC2A Clear Dual-Cure Semi-Flexible Adhesive WCC2A is a clear, non-yellowing, dual-cure (UV and Heat) nameplate coating that is ideal for applications that require a glossy, "lens-like" finish. This photopolymer will also offer low shrinkage d.. |
|||
Adhesive Bond Strength | 5.52 MPa | 800 psi | |
Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming 56C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, high electrical conductivity, epoxy adhesive. Excellent thermal conductivity. Require.. |
|||
Adhesive Bond Strength | 5.52 MPa | 800 psi | |
Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy AdhesiveTwo component, nickel filled, electrically conductive epoxy adhesive. Room temperature cure. Good ba.. |
|||
Adhesive Bond Strength | >= 5.52 MPa | >= 800 psi | shear, Al/Al, after 30 days water immersion |
Master Bond EP21TDCSLO Two Component Silver Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCS-LO is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rap.. |
|||
Adhesive Bond Strength | 5.52 MPa | 800 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Adhesive Bond Strength | 5.52 MPa @Temperature 82.2 °C |
800 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-12 Epoxy Adhesive, at 2:3 Mix Ratio Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati.. |