Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 8.00 - 10.0 MPa | 1160 - 1450 psi | Zinc, Shear; ISO 4587 |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 8.00 MPa | 1160 psi | Zinc, Shear; ISO 4587 |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 - 12.0 MPa | 1160 - 1740 psi | Mild steel, Shear |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Adhesive Bond Strength | 8.00 - 12.0 MPa | 1160 - 1740 psi | Mild steel, Shear; ASTM D1002 |
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Glass/steel, Shear |
Permabond UV670 UV-curable Adhesive PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met.. |
|||
Adhesive Bond Strength | 8.00 - 10.0 MPa | 1160 - 1450 psi | Zinc, Shear |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Adhesive Bond Strength | 8.00 MPa | 1160 psi | steel collar and pin shear; ISO 10123 |
Permabond MH199 Anaerobic Gasketmaker Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Adhesive Bond Strength | 8.00 MPa | 1160 psi | Zinc, Shear; ISO 4587 |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 MPa | 1160 psi | Zinc, Shear; ISO 4587 |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 MPa | 1160 psi | steel collar and pin shear; ISO 10123 |
Permabond A025 Anaerobic Retainer Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for ap.. |
|||
Adhesive Bond Strength | 8.00 MPa | 1160 psi | Zinc, Shear; ISO 4587 |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 8.00 - 9.00 MPa | 1160 - 1310 psi | Aluminum, Shear; ISO 4587 |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |