Polymer Property : Adhesive Bond Strength = 798 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.50 MPa
798 psi
PVC, Shear; ISO 4587
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..