Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 42.1 MPa | 6100 psi | lbs.; NEMA 11.11 |
Glastic 1130 Angles, Channels, and Structural Shapes Information provided by Glastic Corporation |
|||
Adhesive Bond Strength | 42.1 MPa @Temperature 25.0 °C |
6100 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-706 Epoxy Adhesive A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent m.. |
|||
Adhesive Bond Strength | 42.1 MPa | 6100 psi | lbs.; NEMA 11.11 |
Glastic GLASGUARD 1130 Corrosion-Resistant Panels GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corr.. |