Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 20.7 - 41.4 MPa | 3000 - 6000 psi | Varies with substrates |
Loctite® Durabond® E-120HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 20.7 - 41.4 MPa | 3000 - 6000 psi | Varies with substrates |
Loctite® Durabond® E-214HP Epoxy Adhesive Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific.. |