Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 6.90 MPa | 1000 psi | Aluminum, Shear; ASTM D1002 |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Adhesive Bond Strength | 6.90 MPa | 1000 psi | Aluminum, Shear; ASTM D1002 |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Adhesive Bond Strength | 6.90 MPa | 1000 psi | Aluminum, Shear; ASTM D1002 |
Permabond 932 Cyanoacrylate PERMABOND 932 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Adhesive Bond Strength | 6.90 MPa | 1000 psi | Aluminum, Shear; ASTM D1002 |
Permabond 935 Cyanoacrylate The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano.. |
|||
Adhesive Bond Strength | 6.90 MPa @Temperature 25.0 °C |
1000 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol EA 9203 Primer Primer enhances adhesion on poorly prepared surfaces. Requires only room temperature drying prior to bond. Use with room-temperature-curing paste adhesives.Applications: Sprayable Metal and Honeyco.. |
|||
Adhesive Bond Strength | 6.90 - 6.90 MPa @Temperature 121 - 121 °C |
1000 - 1000 psi @Temperature 250 - 250 °F |
Average value: 6.90 MPa Grade Count:1 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |