Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.0427 MPa | 6.20 psi | Arlon SQA-TMS-011 |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Adhesive Bond Strength | 0.0427 MPa | 6.20 psi | Arlon SQA-TMS-011 |
Arlon 51141R020 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Adhesive Bond Strength | 0.0427 MPa | 6.20 psi | ASTM D624 |
Arlon 55276R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |