Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 34.5 MPa | 5000 psi | Varies with substrates |
Loctite® 3292 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Adhesive Bond Strength | 34.5 MPa | 5000 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc.. |
|||
Adhesive Bond Strength | 34.5 MPa | 5000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 970-3 Room Temperature Cure General Purpose Adhesive TRA-BOND 970-3 general purpose adhesive is a non-flowing blue paste. This adhesive cures at room temperature. This adhesive is available in kits with a mix ratio of 100 parts A to 74 parts B or prem.. |
|||
Adhesive Bond Strength | 34.5 MPa | 5000 psi | Steel-Steel; after optimum cure |
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati.. |
|||
Adhesive Bond Strength | 34.5 MPa | 5000 psi | Steel-Steel; after optimum cure |
Armstrong C-7/W Epoxy Adhesive, 2:3 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |