Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 5.50 MPa | 798 psi | PVC, Shear; ISO 4587 |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |