Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 22.1 MPa | 3200 psi | |
Resin Technology Group 350 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 350 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | |
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | |
Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | |
Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Al/Al |
Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications whe.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Epoxy HP 250, Straw Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Steel-Steel; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 406 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 409 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 410 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 414 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 422 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 4471 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 499 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® PRISM® 411 Clear Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® PRISM® 454 Instant Adhesive Gel Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® Tak Pak® 382 Instant Adhesive Cyanoacrylate Bonding Adhesives and Gasketing and Wire TackingLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® Tak Pak® 444 Instant Adhesive Cyanoacrylate Bonding Adhesives and Gasketing and Wire TackersLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of.. |
|||
Adhesive Bond Strength | 22.1 MPa @Temperature -54.4 °C |
3200 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-12-T Epoxy Adhesive Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® 416 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 22.1 MPa | 3200 psi | Grit blasted steel |
Loctite® PRISM® 401 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |