Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 30.3 MPa @Temperature -54.4 °C |
4400 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-701 Epoxy Adhesive A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond.. |