Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 3.45 MPa | 500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |
|||
Adhesive Bond Strength | 3.45 MPa | 500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 813J01 Silicone Encapsulant TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation.. |
|||
Adhesive Bond Strength | 3.45 - 13.8 MPa | 500 - 2000 psi | Varies with substrates |
Loctite® Durabond® U-10FL Urethane Adhesive Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap.. |