Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.0214 MPa | 3.10 psi | Arlon SQA-TMS-011 |
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Adhesive Bond Strength | 0.0214 MPa | 3.10 psi | MIL-I-46852C |