Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 12.0 - 18.0 MPa | 1740 - 2610 psi | Zinc, Shear |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Adhesive Bond Strength | 12.0 - 18.0 MPa | 1740 - 2610 psi | Zinc Plated after 24 hours, Shear |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Adhesive Bond Strength | 12.0 - 18.0 MPa | 1740 - 2610 psi | Zinc Plated after 24 hours, Shear |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Adhesive Bond Strength | 16.0 - 18.0 MPa | 2320 - 2610 psi | Aluminum, Shear; ISO 4587 |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |