Polymer Property : Adhesive Bond Strength = 2370 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 16.3 MPa
>= 2370 psi
ASTM D4541
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating
Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres..