Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 16.2 MPa | 2350 psi | Lap shear, alum to alum, 1 hr @ 100°C |
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and.. |
|||
Adhesive Bond Strength | 16.2 MPa | 2350 psi | Steel-Steel; after optimum cure |
Armstrong A-5/A Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 16.2 MPa @Temperature 82.2 °C |
2350 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-1/E Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Adhesive Bond Strength | 16.2 MPa @Temperature 25.0 °C |
2350 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-1/H20 Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Adhesive Bond Strength | 16.2 MPa @Temperature 82.2 °C |
2350 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-3/E Epoxy Adhesive A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,.. |