Mechanical Properties Metric English Comments
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Adhesive Bond Strength 15.9 - 27.6 MPa
2300 - 4000 psi
Average value: 20.2 MPa Grade Count:4
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear, alum to alum, 1 hr @ 65°C
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive
TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t..
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive
TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi..
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear, alum to alum, 1 hr @ 65°C
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive
TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c..
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Tra-Con Tra-Bond 216E02 Encapsulant for "Fill" Applications
TRA-BOND 216E02 is a two-part epoxy adhesive developed specifically for underfill and encapsulating applications where the combination of excellent mechanical, thermal and electrical properties are ..
Adhesive Bond Strength 15.9 MPa
2300 psi
Adhesive tensile shear strength; ASTM D1002
Devcon Wear Guard (High Temp) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap Shear Strength
Epoxyset Epoxibond EB-347 Low Expansion Epoxy Adhesive
EB-347 is a highly filled, low coefficient expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensiona..
Adhesive Bond Strength 15.9 MPa

@Temperature 82.2 °C
2300 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-1/V Epoxy Adhesive
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El..
Adhesive Bond Strength 15.9 MPa

@Temperature -54.4 °C
2300 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-2/E Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..
Adhesive Bond Strength 15.9 MPa

@Temperature 82.2 °C
2300 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-271 Epoxy Adhesive
A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled ..
Adhesive Bond Strength 15.9 MPa

@Temperature -54.4 °C
2300 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-271 Epoxy Adhesive
A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled ..
Adhesive Bond Strength 15.9 MPa

@Temperature -54.4 °C
2300 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-40 Epoxy Adhesive
Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re..
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive
Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..