Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 14.0 - 17.0 MPa | 2030 - 2470 psi | Glass/steel, Shear |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |