Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.1 MPa | 2190 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive SD, Off-White Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 15.1 MPa | 2190 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond FDA26 Food and Drug Application Epoxy Adhesive Information provided by Tra-Con Inc. |