Polymer Property : Adhesive Bond Strength = 1160 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.00 - 10.0 MPa
1160 - 1450 psi
Zinc, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Adhesive Bond Strength 8.00 MPa
1160 psi
Zinc, Shear; ISO 4587
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Mild steel, Shear
Permabond ET510 Epoxy Resin
PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
Adhesive Bond Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Mild steel, Shear; ASTM D1002
Permabond ET515 Epoxy Resin
PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Glass/steel, Shear
Permabond UV670 UV-curable Adhesive
PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met..
Adhesive Bond Strength 8.00 - 10.0 MPa
1160 - 1450 psi
Zinc, Shear
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Adhesive Bond Strength 8.00 MPa
1160 psi
steel collar and pin shear; ISO 10123
Permabond MH199 Anaerobic Gasketmaker
Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po..
Adhesive Bond Strength 8.00 MPa
1160 psi
Zinc, Shear; ISO 4587
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 MPa
1160 psi
Zinc, Shear; ISO 4587
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 943 Cyanoacrylate, low odor
PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 MPa
1160 psi
steel collar and pin shear; ISO 10123
Permabond A025 Anaerobic Retainer
Permabond® A025 is an anaerobic adhesive formulated to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It has been designed for ap..
Adhesive Bond Strength 8.00 MPa
1160 psi
Zinc, Shear; ISO 4587
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Aluminum, Shear; ISO 4587
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..